Influence of surface oxidation on the morphological and crystallographic structure of multi-walled carbon nanotubes via different oxidants
Abstract
Abstract
In this paper, three kinds of multi-walled carbon nanotubes (MWCNTs) with different diameters (outer diameters: 10 to 20, 30 to 50, and >50 nm) and special surface areas (200, 60, and 40 m
2
/g, respectively) were oxidized in commonly used liquid oxidizers: (1) concentrated nitric acid, (2) a mixture of nitric + sulfuric acids (
V
:
V
, 1:3), (3) hydrogen peroxide, (4) a mixture of hydrogen peroxide + sulfuric acid (
V
:
V
, 1:1), and (5) acidic potassium permanganate. Morphology of the pristine and oxidized MWCNTs was characterized by scanning electron microscopy which provides sufficient resolution for direct visualization of their outer diameter distribution. Full width at half maximum (FWHM) in the X-ray diffraction (XRD) investigation of the MWCNT samples before and after the oxidation process was measured. After treatment with oxidants, a clear decrease in nanotube diameters along the tube walls was observed. Decrease in the degree of crystallites started with the FWHM widening of the XRD diffraction peaks. The particle (crystallite) size (
d
002
) calculated by Bragg's law and Scherrer equation increased depending on the kind of oxidants; the procedure can be performed using a mixture of HNO
3
+ H
2
SO
4
on the surface of the MWCNTs with an outer diameter of 10 to 20nm. However, similar are the diffraction patterns of pristine and oxidized MWCNTs. Therefore, the MWCNTs that underwent oxidation process were able to preserve the first features of their structures, even though some narrowing of outer diameters and decreases in crystallites appeared. Nevertheless, the structure of MWCNTs still remains intact to be used as oxidized nanotubes in most applications.
Keywords
- Multi-walled carbon nanotube,
- Surface functionalization,
- Morphology,
- Crystallographic structure
References
- Ilya et al. (2012) Oxidation behavior of multiwall carbon nanotubes with different diameters and morphology (pp. 6272-6280) https://doi.org/10.1016/j.apsusc.2012.03.021
- Chen et al. (2012) Influence of surface functionalization via chemical oxidation on the properties of carbon nanotubes (pp. 32-38) https://doi.org/10.1016/j.jcis.2011.12.073
- Datsyuk et al. (2008) Chemical oxidation of multiwalled carbon nanotubes (pp. 833-840) https://doi.org/10.1016/j.carbon.2008.02.012
- Avilés et al. (2009) Evaluation of mild acid oxidation treatments for MWCNT functionalization (pp. 2970-2975) https://doi.org/10.1016/j.carbon.2009.06.044
- Dandekar et al. (1998) Characterization of activated carbon, graphitized carbon fibers and synthetic diamond powder using TPD and DRIFTS (pp. 1821-1831) https://doi.org/10.1016/S0008-6223(98)00154-7
- Pereira et al. (2010) Characterization of carbon nanotube 3D-structures infused with low viscosity epoxy resin system (pp. 2252-2257) https://doi.org/10.1016/j.compstruct.2009.08.009
- Tsang et al. (1994) A simple chemical method of opening and filling carbon nanotubes 372(6502) (pp. 59-62) https://doi.org/10.1038/372159a0
- Moreno-Castilla et al. (1998) Effects of non-oxidant and oxidant acid treatments on the surface properties of an activated carbon with very low ash content (pp. 145-151) https://doi.org/10.1016/S0008-6223(97)00171-1
- Zhang et al. (2003) Effect of chemical oxidation on the structure of single-walled carbon nanotubes (pp. 3712-3718) https://doi.org/10.1021/jp027500u
- Aksoylu et al. (2001) The effects of different activated carbon supports and support modifications on the properties of Pt/AC catalysts (pp. 175-185) https://doi.org/10.1016/S0008-6223(00)00102-0
- Esumi et al. (1995) Chemical treatment of carbon nanotubes 34(2) (pp. 279-281) https://doi.org/10.1016/0008-6223(96)83349-5
- Figueiredo et al. (2007) Characterization of active sites on carbon catalysts (pp. 4110-4115) https://doi.org/10.1021/ie061071v
- Chen et al. (1998) Solution properties of single-walled carbon nanotubes 282(5386) (pp. 95-98) https://doi.org/10.1126/science.282.5386.95
- Cuervo et al. (2008) Modification of the adsorption properties of high surface area graphites by oxygen functional groups (pp. 2096-2106) https://doi.org/10.1016/j.carbon.2008.08.025
- Zhao et al. (2004) Synthesis and properties of a water-soluble single-walled carbon nanotube-poly(maminobenzene sulfonic acid) graft copolymer 14(1) (pp. 71-76) https://doi.org/10.1002/adfm.200304440
- Osorio et al. (2008) H2SO4/HNO3/HCl—functionalization and its effect on dispersion of carbon nanotubes (pp. 2485-2489) https://doi.org/10.1016/j.apsusc.2008.07.144
- Lin et al. (2006) Functionalizing multi-walled carbon nanotubes with poly(oxyalkylene)- amidoamines 17(13) (pp. 3197-3203) https://doi.org/10.1088/0957-4484/17/13/020
- Liang et al. (2005) Preparation and characterization of multi-walled carbon nanotubes supported PtRu catalysts for proton exchange membrane fuel cells (pp. 3144-3152) https://doi.org/10.1016/j.carbon.2005.06.017
- Nobili et al. (1990) Characterization of electrophoretic fractions of humic substances with different electrofocusing behaviour 150(5) (pp. 763-770) https://doi.org/10.1097/00010694-199011000-00002
- Ötvös et al. (2006) Surface oxygen complexes as governors of neopentane sorption in multiwalled carbon nanotubes (pp. 1665-1672) https://doi.org/10.1016/j.carbon.2006.01.005
- Figueiredo et al. (1999) Modification of the surface chemistry of activated carbons (pp. 1379-1389) https://doi.org/10.1016/S0008-6223(98)00333-9
- Tran et al. (2007) Thermal oxidative cutting of multi-walled carbon nanotubes 45(12) (pp. 2341-2350) https://doi.org/10.1016/j.carbon.2007.07.012
- Toebes et al. (2004) The influence of oxidation on the texture and the number of oxygen-containing surface groups of carbon nanofibers (pp. 307-315) https://doi.org/10.1016/j.carbon.2003.10.036
- Ajayan et al. (1993) Opening carbon nanotubes with oxygen and implications for filling 362(6420) (pp. 522-525) https://doi.org/10.1038/362522a0
- Barroso-Bujans et al. (2007) Degree of functionalization of carbon nanofibers with benzenesulfonic groups in an acid medium (pp. 1669-1678) https://doi.org/10.1016/j.carbon.2007.03.039
- Hu et al. (2003) Nitric acid purification of single-walled carbon nanotubes 107(50) (pp. 13838-13842)
- Yu-Chun et al. (2011) The influence of treatment duration on multi-walled carbon nanotubes functionalized by H2SO4/HNO3 oxidation (pp. 2401-2410) https://doi.org/10.1016/j.apsusc.2010.09.110
- Wang et al. (2007) Adsorption of fulvic acids from aqueous solutions by carbon nanotubes 82(8) (pp. 698-704) https://doi.org/10.1002/jctb.1708
- Li et al. (2008) Oxidation of single-walled carbon nanotubes in dilute aqueous solutions by ozone as affected by ultrasound (pp. 466-475) https://doi.org/10.1016/j.carbon.2007.12.012
10.1186/2193-8865-3-73